Physical Properties
C92600 Commercial Leaded Tin Bronze

  US Customary Metric
Melting Point - Liquidus 1800 F 982 C
Melting Point - Solidus 1550 F 843 C
Density 0.315 lb/in3 at 68 F 8.72 gm/cm3 @ 20 C
Specific Gravity 8.72 8.72
Electrical Resistivity 115.7 ohms-cmil/ft @ 68 F 19.23 microhm-cm @ 20 C
Electrical Conductivity 9 %IACS @ 68 F 0.052 MegaSiemens/cm @ 20 C
Coefficient of Thermal Expansion 10.0 ·10-6 per oF (68-392 F) 18.0 ·10-6 per oC (20-200 C)
Specific Heat Capacity 0.09 Btu/lb/oF at 68 F 377.1 J/kg · oK at 293 K
Modulas of Elasticity in Tension 15000 ksi 103400 MPa

Common Fabrication Processes

Casting

Fabrication Properties

Joining Technique Suitability
Soldering Excellent
Brazing Good
Oxyacetylene Welding Not Recommended
Gas Shielded Arc Welding Not Recommended
Coated Metal Arc Welding Not Recommended
Machinability Rating 40